Vai al contenuto principale della pagina
| Autore: |
Buckalew William H.
|
| Titolo: |
Response of rubber insulation materials to monoenergetic electron irradiations / / W. H. Buckalew, F. J. Wyant, G. J. Lockwood
|
| Pubblicazione: | Washington, DC : , : Electrical Engineering Branch, Division of Engineering Technology, Office of Nuclear Regulatory Research, U.S. Nuclear Regulatory Commission, , 1983 |
| Descrizione fisica: | 1 online resource (ix, 51 pages) : illustrations |
| Soggetto topico: | Pressurized water reactors - Loss of coolant |
| Nuclear reactors - Materials - United States - Testing | |
| Ethylene-propylene rubber | |
| Persona (resp. second.): | WyantFrancis J. |
| LockwoodGrant J. | |
| Note generali: | "Printed November 1983"--Cover. |
| "This report documents a part of the Qualification Testing Evaluation (QTE) Program being conducted by Sandia National Laboratories"--Cover. | |
| "P 2900-Q(6-82)"--Cover. | |
| "NUREG/CR-3532; SAND83-2098; RV." | |
| Nota di bibliografia: | Includes bibliographical references (pages 17-18). |
| Titolo autorizzato: | Response of rubber insulation materials to monoenergetic electron irradiations ![]() |
| Formato: | Materiale a stampa |
| Livello bibliografico | Monografia |
| Lingua di pubblicazione: | Inglese |
| Record Nr.: | 9910706519403321 |
| Lo trovi qui: | Univ. Federico II |
| Opac: | Controlla la disponibilità qui |