LEADER 02157oam 2200601 450 001 9910713665403321 005 20200623121320.0 035 $a(CKB)5470000002503018 035 $a(OCoLC)1127388959 035 $a(EXLCZ)995470000002503018 100 $a20191113d1928 ua 0 101 0 $aeng 135 $aurbn||||||||| 181 $ctxt$2rdacontent 182 $cc$2rdamedia 183 $acr$2rdacarrier 200 10$aCorrosion embrittlement of duralumin$hIII$iEffect of the previous treatment of sheet material on the susceptibility to this type of corrosion /$fby Henry S. Rawdon 210 1$aWashington, [D.C.] :$cNational Advisory Committee for Aeronautics,$d1928. 215 $a1 online resource (24 pages, 6 unnumbered pages) $cillustrations 225 1 $aTechnical notes / National Advisory Committee for Aeronautics ;$vNo. 284 300 $a"April 1928." 300 $aNo Federal Depository Library Program (FDLP) item number. 320 $aIncludes bibliographical references (page 24). 517 3 $aEffect of the previous treatment of sheet material on the susceptibility to this type of corrosion 606 $aDuralumin$xEmbrittlement 606 $aAluminum alloys 606 $aAlloys$xCorrosion 606 $aAlloys$xEffect of temperature on 606 $aAlloys$xHeat treatment 606 $aAlloys$xCorrosion$2fast 606 $aAlloys$xHeat treatment$2fast 606 $aAluminum alloys$2fast 615 0$aDuralumin$xEmbrittlement. 615 0$aAluminum alloys. 615 0$aAlloys$xCorrosion. 615 0$aAlloys$xEffect of temperature on. 615 0$aAlloys$xHeat treatment. 615 7$aAlloys$xCorrosion. 615 7$aAlloys$xHeat treatment. 615 7$aAluminum alloys. 700 $aRawdon$b Henry S.$f1880-1954,$018605 712 02$aUnited States.$bNational Advisory Committee for Aeronautics, 801 0$bTRAAL 801 1$bTRAAL 801 2$bTRAAL 801 2$bOCLCO 801 2$bOCLCF 801 2$bGZS 801 2$bGPO 906 $aBOOK 912 $a9910713665403321 996 $aCorrosion embrittlement of duralumin$93458779 997 $aUNINA