LEADER 01412aam 2200397I 450 001 9910710510903321 005 20160705110709.0 024 8 $aGOVPUB-C13-7b6c2832400638c1399eaf5dc0036b65 035 $a(CKB)5470000002478192 035 $a(OCoLC)953032954 035 $a(EXLCZ)995470000002478192 100 $a20160705d1988 ua 0 101 0 $aeng 181 $2rdacontent 182 $2rdamedia 183 $2rdacarrier 200 10$aReport of roof inspection $epartial delamination of adhesive-bonded seams at an army facility /$fWalter J. Rossiter Jr.; James F. Seiler Jr 210 1$aGaithersburg, MD :$cU.S. Dept. of Commerce, National Institute of Standards and Technology,$d1988. 215 $a1 online resource 225 1 $aNISTIR ;$v88-3893 300 $a1988. 300 $aContributed record: Metadata reviewed, not verified. Some fields updated by batch processes. 300 $aTitle from PDF title page. 320 $aIncludes bibliographical references. 517 $aReport of roof inspection 700 $aRossiter$b Walter J$01382014 701 $aRossiter$b Walter J$01382014 701 $aSeiler$b James F.$cJr.$01392803 712 02$aNational Institute of Standards and Technology (U.S.) 801 0$bNBS 801 1$bNBS 801 2$bGPO 906 $aBOOK 912 $a9910710510903321 996 $aReport of roof inspection$93504725 997 $aUNINA