LEADER 01419aam 2200409I 450 001 9910710052003321 005 20151118015324.0 024 8 $aGOVPUB-C13-5470bb12b87ac740595a2c002c6e58bc 035 $a(CKB)5470000002475757 035 $a(OCoLC)929881633 035 $a(EXLCZ)995470000002475757 100 $a20151118d1975 ua 0 101 0 $aeng 181 $2rdacontent 182 $2rdamedia 183 $2rdacarrier 200 10$aStrength degradation of brittle surfaces $eblunt indenters /$fB. R. Lawn; S. M. Wiederhorn; H. H. Johnson 210 1$aGaithersburg, MD :$cU.S. Dept. of Commerce, National Institute of Standards and Technology,$d1975. 215 $a1 online resource 225 1 $aNBSIR ;$v75-664 300 $a1975. 300 $aContributed record: Metadata reviewed, not verified. Some fields updated by batch processes. 300 $aTitle from PDF title page. 320 $aIncludes bibliographical references. 517 $aStrength degradation of brittle surfaces 700 $aLawn$b Brian R$043353 701 $aJohnson$b H. H$01406610 701 $aLawn$b Brian R$043353 701 $aWiederhorn$b S. M$01118568 712 02$aUnited States.$bNational Bureau of Standards. 801 0$bNBS 801 1$bNBS 801 2$bGPO 906 $aBOOK 912 $a9910710052003321 996 $aStrength degradation of brittle surfaces$93486006 997 $aUNINA