LEADER 01671nam 2200469Ia 450 001 9910699376403321 005 20230902162209.0 035 $a(CKB)5470000002402150 035 $a(OCoLC)586063305 035 $a(EXLCZ)995470000002402150 100 $a20100329d2009 ua 0 101 0 $aeng 135 $aurcn||||||||| 181 $ctxt$2rdacontent 182 $cc$2rdamedia 183 $acr$2rdacarrier 200 00$aUse of liquid metal embrittlement (LME) for controlled fracture$b[electronic resource] /$fJames C. Hirvonen ... [and others] ; William S. de Rosset 210 1$aAberdeen Proving Ground, MD :$cArmy Research Laboratory,$d[2009] 215 $a1 online resource (vi, 40 pages) $cillustrations (some color) 225 1 $aARL-TR ;$v4976 300 $a"September 2009." 300 $aTitle from PDF title screen (viewed on Mar. 29, 2010). 320 $aincludes bibliographical references (pages 22-23). 410 0$aARL-TR (Aberdeen Proving Ground, Md.) ;$v4976. 517 $aUse of liquid metal embrittlement 606 $aMetals$xEmbrittlement 606 $aLiquid metals 606 $aSteel$xFracture 606 $aNotched bar testing 615 0$aMetals$xEmbrittlement. 615 0$aLiquid metals. 615 0$aSteel$xFracture. 615 0$aNotched bar testing. 701 $aHirvonen$b J. K$g(James Karsten),$f1943-$01413360 701 $aDe Rosset$b William S$01391666 712 02$aU.S. Army Research Laboratory. 801 0$bGPO 801 1$bGPO 906 $aBOOK 912 $a9910699376403321 996 $aUse of liquid metal embrittlement (LME) for controlled fracture$93509606 997 $aUNINA