LEADER 01584oam 2200445Ia 450 001 9910698757303321 005 20090710103636.0 035 $a(CKB)5470000002396282 035 $a(OCoLC)318684958 035 $a(EXLCZ)995470000002396282 100 $a20090122d2008 ka 0 101 0 $aeng 135 $aurbn||||||||| 181 $ctxt$2rdacontent 182 $cc$2rdamedia 183 $acr$2rdacarrier 200 10$aLandau-Devonshire parameters for the tunable paraelectric material BaTi.9(Sc,Ta).05O3$b[electronic resource] /$fby Virginia Miller and Frank Crowne 210 1$aAdelphi, MD :$cArmy Research Laboratory,$d[2008] 215 $aiv, 14 pages $cdigital, PDF file 225 1 $aARL-TR ;$v4403 300 $aTitle from title screen (viewed July 10, 2009). 300 $a"March 2008." 320 $aIncludes bibliographical references (page 10). 517 $aLandau-Devonshire parameters for the tunable paraelectric material BaTi.9 606 $aTransition metals 606 $aFerroelectricity$xMathematical models 606 $aTransition temperature 615 0$aTransition metals. 615 0$aFerroelectricity$xMathematical models. 615 0$aTransition temperature. 700 $aMiller$b Virginia$01220279 701 $aCrowne$b Frank$01400801 712 02$aU.S. Army Research Laboratory. 801 0$bDTICE 801 1$bDTICE 801 2$bGPO 906 $aBOOK 912 $a9910698757303321 996 $aLandau-Devonshire parameters for the tunable paraelectric material BaTi.9(Sc,Ta).05O3$93487337 997 $aUNINA